GH3230
| Density | 8.3 g/cc | Melting point | 1370-1420°C |
| Thermal conductivity | 12 W/mK | Electrical resistivity | 70 μΩ-cm |
| Coefficient of thermal expansion | 12.5 x 10^-6 /K | ||
Mechanical properties
| Hardness (HRC) | Solution annealed: 37 HRC | ||
| Hardness (HRC) | Peak aged: 52-58 HRC | ||
| Condition | Tensile strength (MPa) | Yield strength (MPa) | Elongation (%) |
| Annealed | 1100 MPa | / | / |
| Aged | 1600-2000 MPa | 1400-1800 MPa | 8-12% |