HA188 (Haynes 188, UNSR 30188)
| Size distribution | 15–53 μm | Hall flow s/50g | ≤25 |
| D10 (μm) | ≥15 | D50 (μm) | 30-40 |
| D90 (μm) | ≤60 | Bulk density g/cm³ | ≥4.80 |
| Tap density g/cm³ | ≥5.30 | Sphericity | / |
Heat treatment recommendation
| Solution Heat Treatment | 1180±20°C/1H/AC | ||
Mechanical properties
| Measuring temperature | Tensile strength (MPa) | Yield strength (MPa) | Elongation (%) |
| 25°C | ≥900 | ≥400 | ≥45 |
| 650°C | ≥650 | ≥280 | ≥50 |
| 900°C | ≥300 | ≥240 | ≥50 |
| 950°C | ≥200 | ≥170 | ≥50 |
| 1000°C | ≥160 | ≥130 | ≥50 |
Returns will be accepted for up to 7 days of Customer’s receipt or tracking number on unopen items. You, as a Customer, are obliged to inform us via email before you return the item.

Global Material Access
Premium metal powders from trusted manufacturers worldwide.

Complete Additive Solutions
Materials, machines, and metal printing services in one place.

Competitive Pricing
Factory-direct sourcing for better value and cost efficiency.

Technical Support & Expertise
Professional guidance for material selection and printing success.